This search combines search strings from the content search (i.e. "Full Text", "Author", "Title", "Abstract", or "Keywords") with "Article Type" and "Publication Date Range" using the AND operator.
Beilstein J. Nanotechnol. 2018, 9, 1995–2014, doi:10.3762/bjnano.9.190
Figure 1: a) Scheme of a MoO3 nanocrystal on MoS2. The AFM tip is firmly positioned on top on the nanocrystal...
Figure 2: a) Example of a nanomanipulation during which half of a nanoparticle is scan-imaged, before the tip...
Figure 3: Dependence of nanoparticle shear stress on the contact area. a) Relative shear stress obtained from...
Figure 4: Front perspective: a snapshot of a MD-simulated frictional interface between a colloidal monolayer ...
Figure 5: a) A graphene nanoribbon manipulated along a Au(111) surface. A probing tip lifts the GNR verticall...
Figure 6: Single-molecule tribology. a) Schematic drawing of the experiment: A single porphyrin molecule is a...
Figure 7: Non-contact friction experiments of NbSe2. At certain voltages and distances, one finds dramaticall...
Figure 8: The “Swiss Nanodragster” (SND), a 4’-(p-tolyl)-2,2’:6’,2”-terpyridine molecule, was moved across an...
Figure 9: Example of a change of conformation potentially triggered at surfaces. a) Trans (1) and cis (2) iso...
Beilstein J. Nanotechnol. 2012, 3, 852–859, doi:10.3762/bjnano.3.96
Figure 1: The two-dimensional material consisting of carbon atoms in honeycomb orientation, graphene (a), los...
Figure 2: AFM measurements of HOPG after hydrogen plasma exposure at 450 °C, where round-shaped blisters appe...
Figure 3: (a) XPS and (b) UPS spectra of the HOPG before exposure, after 30 min of exposure and after an anne...
Figure 4: (a) STM images of the HOPG after 5 min of hydrogen plasma exposure at 450 °C and (b) after an annea...
Figure 5: Top-view STM image of the surface consisting of various atomic-scale patterns where a very low defe...